特性: 符合 ECO,流动性高
机构评级: EU Eco
加工方法: 注射成型
多点数据: Coefficient of Thermal Expansion vs. Temperature (ASTM E831),Flexural DMA (ASTM D4065),Instrumented Impact (Energy) (ASTM D3763),Instrumented Impact (Load) (ASTM D3763),Pressure-Volume-Temperature (PVT - Zoller Method),Shear DMA (ASTM D4065),Specific Heat vs. Temperature (ASTM D3417),Tensile Fatigue,Tensile Stress vs. Strain (ASTM D638),Thermal Conductivity vs. Temperature (ASTM E1530),Viscosity vs. Shear Rate (ASTM D3835)
- 比重 1.26 g/cm³ ASTM D792
- 背压 MPa
- 排气孔深度 mm
- 料筒前部温度 °C
- 加工(熔体)温度 °C
- 无缺口悬臂梁冲击 2100 J/m ASTM D4812
- 干燥温度 135 °C
- 排气孔深度 mm
- UL 阻燃等级 UL 94
- 模具温度 °C