Product TextsVESTAMID® X7293 nc Properties of compounds based on Polyamide 12 vary little with changingParts made of this semicrystalline material are charac- of deflection under load (1.80 MPa)
45°CISO 75-1/-2
温度负荷变形(Temp. of deflection under load) (0.45 MPa)100°CISO 75-1/-2
维卡软化温度(50℃/ h的50N)Vicat softening temperature130°CISO 306
COEFF线性热(Coeff. of linear therm. expansion) (parallel)180E-6/KISO 11359-1/-2
COEFF线性热(Coeff. of linear therm. expansion) (normal)180E-6/KISO 11359-1/-2
燃烧性(球压痕硬度(Burning behav)). at 1.5 mm nom. thickn.HBclassIEC 60695-11-10
厚度测试(Thickness tested)1.6mmIEC 60695-11-10
燃烧性(球压痕硬度(Burning behav)). at thickness hHBclassIEC 60695-11-10
厚度测试(Thickness tested)3.2mmIEC 60695-11-10
电气性能(Electrical properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
相对介电常数(Relative permittivity) (100Hz)11-IEC 60250
相对介电常数(Relative permittivity) (1MHz)4.6-IEC 60250
耗散因数(耗散因数(Dissipation factor)) (100Hz)2000E-4IEC 60250
耗散因数(耗散因数(Dissipation factor)) (1MHz)1900E-4IEC 60250
体积电阻率(Volume resistivity)1E10Ohm*mIEC 60093
电气强度(Electric strength)30kV/mmIEC 60243-1
相比漏电起痕指数(Comparative tracking index)600-IEC 60112
其他属性(Other properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
密度(Density)1020kg/m³ISO 1183
Test specimen production值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
Injection Molding, melt temperature240°CISO 294
Injection Molding, mold temperature80°CISO 10724
Injection Molding, injection velocity200mm/sISO 294
Injection Molding, pressure at hold70MPaISO 294
CharacteristicsProcessingInjection Molding, Profile Extrusion, Other ExtrusionDelivery formPelletsAdditivesLubricantsSpecial CharacteristicsHigh impact or impact modified, Light stabilized or stable to light, U.V. stabilized or stable to weather, Heat stabilized or stable to heatRegional AvailabilityNorth America, Europe, Asia Pacific, South and Central America, Near East/AfricaOther text informationInjection moldingPREPROCESSING INFORMATION1 % The drying time is dependentAt a drying temperature of 80°C we recommend, depending on the waterFresh air dryers are acceptable, better would be a dry air orPlease note our product literature, plasticized resins can lose plasticizer during 1 % The drying time is dependent on the drying temperature. At a drying temperature of 80°C we recommend, depending on the waterFresh air dryers are acceptable, better would be a dry air orPlease note our product literature, plasticized resins can lose plasticizer during drying.1 % The drying time is dependentAt a drying temperature of 80°C we recommend, depending on the waterFresh air dryers are acceptable, better would be a dry air orPlease note our product literature, plasticized resins can lose plasticizer du ISO 1817 Liquid C) (23°C)[/td][/tr][tr][td] ISO 1817 Liquid 4) (23°C)[/td][/tr][tr][td] ISO 1817 Liquid F) (23°C)[/td][/tr][tr][td] ISO 1817 Liquid F) (90°C)[/td][/tr][tr][td] 4 Brake fluid (120°C)[/td][/tr][tr][td] .
[/td][/tr][/table]

转载请注明: 转自中国塑胶原料之家 http://www.su-jiao.com/wuxingbiao/

本文链接: http://www.su-jiao.com/wuxingbiao/show-101056.html

免责声明: 本文 VESTAMID® X7293 nc (nf)|PA12-I|Evonik Industries 仅代表作者个人观点,中国塑胶原料之家无关。中国塑胶原料之家网所转载的内容,其版权均由原作者和资料提供方所拥有!如因作品版权问题需要处理,请与我们联络

塑胶原料之家,专业塑料网站、原料报价网站,免费发布塑胶供求信息。塑胶原料之家为您提供塑料供应、塑料求购、塑料行情、塑料展会、塑料原料资讯服务。

2008-2015 塑料|塑胶原料|物性表大全|UL黄卡|SGS报告查询|最新价格--塑胶原料之家

沪ICP备15027283号-4