Product TextsISO 9988: POM-H,MNR,5-2  Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating and available in a variety of colours and speciality grades. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-17 kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.  It has improved processing thermal stability, good mechanical properties, and low volatile emissions.g. consumer electronics parts, zippers.05
kg-
模具收缩(Mold Shrinkage) (MD)0.0175mm/mmASTM D 955
模具收缩(Mold Shrinkage) (TD)0.0185mm/mmASTM D 955
密度(Density) (73°F)1420kg/m³ASTM D 792
吸水率(Water Absorption) (24hr)0.43%ASTM D 570
吸水率(Water Absorption) (Equilibrium)1.4%ASTM D 570
流变性能(Rheological properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
熔体体积流动速率(Melt volume-flow rate) (MVR)21cm³/10minISO 1133
温度(Temperature)190°CISO 1133
负载(Load)2.16kgISO 1133
成型收缩(Molding shrinkage) (parallel)2.1%ISO 294-4, 2577
成型收缩(Molding shrinkage) (normal)2.0%ISO 294-4, 2577
机械性能(机械性能(Mechanical properties))值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
拉伸模量(Tensile Modulus)3200MPaISO 527-1/-2
屈服应力(Yield stress)71MPaISO 527-1/-2
屈服应变(Yield strain)12%ISO 527-1/-2
断裂拉伸应变(Nominal strain at break)25%ISO 527-1/-2
Tensile creep modulus (1h)2800MPaISO 899-1
Tensile creep modulus (1000h)1500MPaISO 899-1
简支梁冲击强度(Charpy impact strength) (+23°C)200kJ/m²ISO 179/1eU
简支梁冲击强度(Charpy impact strength) (-30°C)200kJ/m²ISO 179/1eU
简支梁缺口冲击强度(Charpy notched impact strength) (+23°C)7kJ/m²ISO 179/1eA
简支梁缺口冲击强度(Charpy notched impact strength) (-30°C)6kJ/m²ISO 179/1eA
ASTM数据(ASTM Data)
拉伸模量(Tensile Modulus)3480MPaASTM D 638
抗拉强度(Tensile Strength) at Yield69MPaASTM D 638
屈服伸长率(Elongation at Yield)11%ASTM D 638
断裂伸长率(Elongation at Break)25%ASTM D 638
弯曲弹性模量(弯曲弹性模量(Flexural Modulus))3240MPaASTM D 790
洛氏硬度(Rockwell Hardness)R 120-ASTM D 785
悬臂梁式冲击切口 (1/8 in)0.069kJ/mASTM D 256
热性能(热性能(Thermal properties))值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
熔化温度(熔化温度(Melting temperature)) (10°C/min)178°CISO 11357-1/-3
温度负荷变形(Temp. of deflection under load) (1.80 MPa)95°CISO 75-1/-2
温度负荷变形(Temp. of deflection under load) (0.45 MPa)165°CISO 75-1/-2
维卡软化温度(50℃/ h的50N)Vicat softening temperature160°CISO 306
COEFF线性热(Coeff. of linear therm. expansion) (parallel)120E-6/KISO 11359-1/-2
COEFF线性热(Coeff. of linear therm. expansion) (normal)120E-6/KISO 11359-1/-2
燃烧性(球压痕硬度(Burning behav)). at 1.5 mm nom. thickn.HBclassIEC 60695-11-10
厚度测试(Thickness tested)1.5mmIEC 60695-11-10
UL 识别(recognition)UL--
燃烧性(球压痕硬度(Burning behav)). at thickness hHBclassIEC 60695-11-10
厚度测试(Thickness tested)0.8mmIEC 60695-11-10
UL 识别(recognition)UL--
Oxygen index23%ISO 4589-1/-2
ASTM数据(ASTM Data)
UL 94 阻燃等级(Flame rating)HB-UL 94
厚度测试(Thickness tested)1.5mm-
DTUL @ 66 psi163°CASTM D 648
DTUL @ 264 psi105°CASTM D 648
熔化温度(Melting 温度(Temperature))178°CASTM D 3418
电气性能(Electrical properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
相对介电常数(Relative permittivity) (100Hz)3.8-IEC 60250
相对介电常数(Relative permittivity) (1MHz)3.8-IEC 60250
耗散因数(耗散因数(Dissipation factor)) (100Hz)180E-4IEC 60250
耗散因数(耗散因数(Dissipation factor)) (1MHz)50E-4IEC 60250
体积电阻率(Volume resistivity)1E12Ohm*mIEC 60093
表面电阻率(Surface resistivity)>1E15OhmIEC 60093
电气强度(Electric strength)32kV/mmIEC 60243-1
相比漏电起痕指数(Comparative tracking index)600-IEC 60112
ASTM数据(ASTM Data)
绝缘强度(Dielectric Strength) (Short Time)17.3kV/mmASTM D 149
耗散因数(Dissipation Factor) (1 MHz)0.006-ASTM D 150
介电常数(Dielectric Constant) (1 MHz)3.6-ASTM D 150
表面电阻率(Surface Resistivity)5E14OhmASTM D 257
体积电阻率(Volume Resistivity)2E14Ohm*cmASTM D 257
其他属性(Other properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
吸水率(Water absorption)1.4%Sim. to ISO 62
吸湿性(Humidity absorption)0.3%Sim. to ISO 62
密度(Density)1420kg/m³ISO 1183
流变计算属性(Rheological calculation properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
密度(Density) of melt1170kg/m³-
熔体热导率(Thermal conductivity of melt)0.22W/(m K)-
规格的热容融化(Spec. heat capacity of melt)3020J/(kg K)-
喷射温度(Ejection temperature)141°C-
Diagrams ISO 1817 Liquid C) (23°C)[/td][/tr][tr][td] ISO 1817 Liquid 4) (23°C)[/td][/tr][tr][td] ISO 1817 Liquid F) (23°C)[/td][/tr][tr][td] ISO 1817 Liquid F) (90°C)[/td][/tr][tr][td] ISO 1817 Liquid F) (>90°C)[/td][/tr][tr][td]Salt solutions[/td][/tr][tr][td] 4 Brake fluid (130°C)[/td][/tr][tr][td] M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from M-Base; this is especially valid for claims of compensation resulting from consequential damages. M-Base explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
[/td][/tr][/table]

转载请注明: 转自中国塑胶原料之家 http://www.su-jiao.com/wuxingbiao/

本文链接: http://www.su-jiao.com/wuxingbiao/show-76035.html

免责声明: 本文 Delrin® 900P NC010|POM|DuPont 仅代表作者个人观点,中国塑胶原料之家无关。中国塑胶原料之家网所转载的内容,其版权均由原作者和资料提供方所拥有!如因作品版权问题需要处理,请与我们联络

塑胶原料之家,专业塑料网站、原料报价网站,免费发布塑胶供求信息。塑胶原料之家为您提供塑料供应、塑料求购、塑料行情、塑料展会、塑料原料资讯服务。

2008-2015 塑料|塑胶原料|物性表大全|UL黄卡|SGS报告查询|最新价格--塑胶原料之家

沪ICP备15027283号-4