加工/物理特性值(Value)单位(Unit)测试标准(Test Standard)
ASTM数据(ASTM Data)
熔体流动指数(Melt Flow Index)8g/10minASTM D 1238
温度(Temperature)230°C-
负载(Load)2.16kg-
密度(Density) (73°F)1060kg/m³ASTM D 792
吸水率(Water Absorption) (24hr)0.02%ASTM D 570
机械性能(机械性能(Mechanical properties))值(Value)单位(Unit)测试标准(Test Standard)
ISO数据
简支梁缺口冲击强度(Charpy notched impact strength) (+23°C)10kJ/m²ISO 179/1eA
ASTM数据(ASTM Data)
抗拉强度(Tensile Strength) at Break75MPaASTM D 638
弯曲弹性模量(弯曲弹性模量(Flexural Modulus))4200MPaASTM D 790
悬臂梁式冲击切口 (1/8 in)0.105kJ/mASTM D 256
热性能(热性能(Thermal properties))值(Value)单位(Unit)测试标准(Test Standard)
ASTM数据(ASTM Data)
UL 94 阻燃等级(Flame rating)HB-UL 94
厚度测试(Thickness tested)3.2mm-
热膨胀系数(Coefficient of Thermal Expansion) (MD)60E-6/KASTM D 696
DTUL @ 264 psi142°CASTM D 648
电气性能(Electrical properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据
相比漏电起痕指数(Comparative tracking index)650-IEC 60112
ASTM数据(ASTM Data)
表面电阻率(Surface Resistivity)1E15OhmASTM D 257
CharacteristicsRegional AvailabilityEurope, South and Central AmericaDisclaimerCopyright M-Base .

转载请注明: 转自中国塑胶原料之家 http://www.su-jiao.com/wuxingbiao/

本文链接: http://www.su-jiao.com/wuxingbiao/show-91090.html

免责声明: 本文 Tecnoprene® HKM41|PP-(GF+T)25|SO.F.TER. 仅代表作者个人观点,中国塑胶原料之家无关。中国塑胶原料之家网所转载的内容,其版权均由原作者和资料提供方所拥有!如因作品版权问题需要处理,请与我们联络

塑胶原料之家,专业塑料网站、原料报价网站,免费发布塑胶供求信息。塑胶原料之家为您提供塑料供应、塑料求购、塑料行情、塑料展会、塑料原料资讯服务。

2008-2015 塑料|塑胶原料|物性表大全|UL黄卡|SGS报告查询|最新价格--塑胶原料之家

沪ICP备15027283号-4