- 弯曲强度 [MPa]: 15.1
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 64 | 64 | Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412 |
Tensile Strength, Ultimate | 15.1 MPa | 2190 psi | Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412 |
Elongation at Break | 340 % | 340 % | Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412 |
100% Modulus | 0.00340 GPa | 0.493 ksi | Cured 10 min at 177°C and Post Cured 24 hr at 232°C; ASTM D412 |
Tear Strength | 28.7 kN/m | 164 pli | Cured 10 min at 177°C and Post Cured 24 hr at 232°C |
Compression Set | 36 % @Temperature 200 °C | 36 % @Temperature 392 °F | Method B, O-rings 70 hr; ASTM D1414 |