- 拉伸强度 [MPa]: 30.23
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 68 | 68 | |
Tensile Strength, Yield | 30.23 MPa | 4384 psi | |
Elongation at Yield | 277 % | 277 % | |
100% Modulus | 0.00466 GPa | 0.676 ksi | |
200% Modulus | 0.01726 GPa | 2.504 ksi | |
Tear Strength | 59.7 kN/m | 341 pli | Die C |
Compression Set | 17 % @Temperature 100 °C, Time 79200 sec | 17 % @Temperature 212 °F, Time 22.0 hour | |
Processing Properties | Metric | English | Comments |
Cure Time | 15.0 min @Temperature 160 °C | 0.250 hour @Temperature 320 °F |