- 拉伸强度 [MPa]: 21.38
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 30 | 30 | |
Tensile Strength, Yield | 21.38 MPa | 3101 psi | |
Elongation at Yield | 641 % | 641 % | |
100% Modulus | 0.000772 GPa | 0.112 ksi | |
200% Modulus | 0.00121 GPa | 0.175 ksi | |
300% Modulus | 0.00171 GPa | 0.248 ksi | |
Tear Strength | 27.3 kN/m | 156 pli | Die C |
Processing Properties | Metric | English | Comments |
Cure Time | 15.0 min @Temperature 149 °C | 0.250 hour @Temperature 300 °F |