- 拉伸强度 [MPa]: 32.4
Mechanical Properties | Metric | English | Comments | ||
---|---|---|---|---|---|
Hardness, Shore A | 64 | 64 | |||
Tensile Strength, Yield | 32.4 MPa | 4700 psi | |||
Elongation at Break | 650 % | 650 % | |||
300% Modulus | 0.008101 GPa | 1.175 ksi | |||
Compression Set | 34 % @Temperature 70.0 °C, Time 79200 sec | 34 % @Temperature 158 °F, Time 22.0 hour | |||
Processing Properties | Metric | English | Comments | ||
Cure Time | 15.0 min @Temperature 166 °C | 0.250 hour @Temperature 330 °F | |||
Descriptive Properties | |||||
500% Modulus (ksi) | 2.7 |