- 拉伸强度 [MPa]: 21.7
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 78 | 78 | |
Tensile Strength, Yield | 21.7 MPa | 3150 psi | |
Elongation at Yield | 473 % | 473 % | |
100% Modulus | 0.009418 GPa | 1.366 ksi | |
200% Modulus | 0.01094 GPa | 1.587 ksi | |
300% Modulus | 0.01249 GPa | 1.812 ksi | |
Tear Strength | 56.2 kN/m | 321 pli | Die C |
Compression Set | 62 % @Temperature 70.0 °C, Time 79200 sec | 62 % @Temperature 158 °F, Time 22.0 hour | |
Processing Properties | Metric | English | Comments |
Cure Time | 20.0 min @Temperature 154 °C | 0.333 hour @Temperature 310 °F | Press cured |