- 密度 [g/cm3]: 1.23
- 拉伸强度 [MPa]: 45.0
- 热变形温度 [℃]: 70.0
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.23 g/cc | 0.0444 lb/in³ | |
Linear Mold Shrinkage, Flow | 0.0020 - 0.0050 cm/cm | 0.0020 - 0.0050 in/in | |
Mechanical Properties | Metric | English | Comments |
Tensile Strength, Yield | 45.0 MPa | 6530 psi | 50 mm/min |
Elongation at Break | >= 50 % | >= 50 % | |
Elongation at Yield | 4.2 % | 4.2 % | |
Tensile Modulus | 1.95 GPa | 283 ksi | 1mm/min |
Charpy Impact Unnotched | NB | NB | |
NB @Temperature -30.0 °C | NB @Temperature -22.0 °F | ||
Charpy Impact, Notched | 1.46 J/cm² | 6.95 ft-lb/in² | |
0.620 J/cm² @Temperature -30.0 °C | 2.95 ft-lb/in² @Temperature -22.0 °F | ||
Electrical Properties | Metric | English | Comments |
Electrical Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | |
Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | |
Dielectric Strength | 16.3 kV/mm | 414 kV/in | |
Dissipation Factor | 0.013 @Frequency 1e+6 Hz | 0.013 @Frequency 1e+6 Hz | |
Comparative Tracking Index | 600 V | 600 V | |
Thermal Properties | Metric | English | Comments |
CTE, linear | 91.0 µm/m-°C @Temperature 20.0 °C | 50.6 µin/in-°F @Temperature 68.0 °F | in flow direction |
CTE, linear, Transverse to Flow | 78.0 µm/m-°C @Temperature 20.0 °C | 43.3 µin/in-°F @Temperature 68.0 °F | |
Specific Heat Capacity | 1.34 J/g-°C | 0.320 BTU/lb-°F | |
Thermal Conductivity | 0.190 W/m-K | 1.32 BTU-in/hr-ft²-°F | |
Deflection Temperature at 0.46 MPa (66 psi) | 70.0 °C | 158 °F | |
Deflection Temperature at 1.8 MPa (264 psi) | 66.0 °C | 151 °F | |
Vicat Softening Point | 77.0 °C | 171 °F | |
Glass Transition Temp, Tg | 83.0 °C | 181 °F | |
Flammability, UL94 | HB @Thickness 1.60 mm | HB @Thickness 0.0630 in | |
HB @Thickness 1.60 mm | HB @Thickness 0.0630 in | ||
HB @Thickness 3.20 mm | HB @Thickness 0.126 in | ||
HB @Thickness 3.20 mm | HB @Thickness 0.126 in | ||
Processing Properties | Metric | English | Comments |
Melt Temperature | 275 - 295 °C | 527 - 563 °F |