- 密度 [g/cm3]: 0.924
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.924 g/cc | 0.0334 lb/in³ | ExxonMobil Method |
Thickness | 50.8 microns | 2.00 mil | |
Antiblock Level | 2000 ppm | 2000 ppm | |
Mechanical Properties | Metric | English | Comments |
Film Tensile Strength at Yield, MD | 11.0 MPa | 1600 psi | ASTM D882 |
Film Tensile Strength at Yield, TD | 11.8 MPa | 1710 psi | ASTM D882 |
Film Elongation at Break, MD | 130 % | 130 % | ASTM D882 |
Film Elongation at Break, TD | 540 % | 540 % | ASTM D882 |
Puncture Energy | 0.859 J | 0.633 ft-lb | ExxonMobil Method |
Elmendorf Tear Strength MD | 510 g | 510 g | ASTM D1922 |
Elmendorf Tear Strength TD | 140 g | 140 g | ASTM D1922 |
Dart drop Test | 170 g | 0.375 lb | ASTM D1709 |
Film Tensile Strength at Break, MD | 25.5 MPa | 3700 psi | ASTM D882 |
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
1% Secant Modulus, MD | 234 MPa | 34000 psi | ASTM D882 |
1% Secant Modulus, TD | 290 MPa | 42000 psi | ASTM D882 |
Thermal Properties | Metric | English | Comments |
Melting Point | 112 °C | 234 °F | Peak Melting Temperature; ExxonMobil Method |
Optical Properties | Metric | English | Comments |
Haze | 9.6 % | 9.6 % | ASTM D1003 |
Gloss | 57 % | 57 % | 45°; ASTM D2457 |