- 密度 [g/cm3]: 2.175
- 弯曲强度 [MPa]: 40.0
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.175 g/cc | 0.07858 lb/in³ | ASTM D792 |
Apparent Bulk Density | 0.370 g/cc | 0.0134 lb/in³ | ASTM D4894 |
Water Absorption | 0.00 % | 0.00 % | ASTM D570 |
Linear Mold Shrinkage | 0.031 cm/cm | 0.031 in/in | Radial shrinkage of 10 cm o.d. sintered rod at 23°C |
Mechanical Properties | Metric | English | Comments |
Tensile Strength, Ultimate | 40.0 MPa | 5800 psi | ASTM D638 |
Elongation at Break | 380 % | 380 % | ASTM D638 |
Coefficient of Friction, Dynamic | 0.060 | 0.060 | ASTM D1894 |
Coefficient of Friction, Static | 0.080 | 0.080 | ASTM D1894 |
Electrical Properties | Metric | English | Comments |
Electrical Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm | ASTM D257 |
Dielectric Constant | 2.1 @Frequency 60.0 - 2.00e+9 Hz | 2.1 @Frequency 60.0 - 2.00e+9 Hz | ASTM D150 |
Dielectric Strength | 70.0 kV/mm | 1780 kV/in | ASTM D149 |
Dissipation Factor | >= 0.00030 @Frequency 60.0 - 2.00e+9 Hz | >= 0.00030 @Frequency 60.0 - 2.00e+9 Hz | ASTM D150 |
Thermal Properties | Metric | English | Comments |
Thermal Conductivity | 0.240 W/m-K | 1.67 BTU-in/hr-ft²-°F | ASTM C177 |
Maximum Service Temperature, Air | 260 °C | 500 °F | Continuous Service |
Flammability, UL94 | V-0 | V-0 | VE-0 |
Oxygen Index | >= 95 % | >= 95 % | ASTM D2863 |