- 密度 [g/cm3]: 0.89
Physical Properties | Metric | English | Comments | ||
---|---|---|---|---|---|
Density | >= 0.890 g/cc | >= 0.0322 lb/in³ | |||
Mechanical Properties | Metric | English | Comments | ||
Hardness, Shore A | 65 | 65 | |||
Hardness, Shore D | 20 | 20 | |||
Thermal Properties | Metric | English | Comments | ||
Maximum Service Temperature, Air | 65.0 °C | 149 °F | |||
Minimum Service Temperature, Air | -30.0 °C | -22.0 °F | |||
Shrinkage | 0.50 - 2.0 % | 0.50 - 2.0 % | |||
Processing Properties | Metric | English | Comments | ||
Rear Barrel Temperature | 150 - 180 °C | 302 - 356 °F | |||
Middle Barrel Temperature | 150 - 180 °C | 302 - 356 °F | |||
Front Barrel Temperature | 150 - 180 °C | 302 - 356 °F | |||
Die Temperature | 140 - 180 °C | 284 - 356 °F | |||
Mold Temperature | 15.0 - 30.0 °C | 59.0 - 86.0 °F | |||
Descriptive Properties | |||||
Acid-Base Resistance | good | ||||
Comp. Ratio | 1.5 - 3.0 | ||||
Compression Set | medium | ||||
Draw Down | 5-10 | ||||
Drying | not necessary | ||||
Injection Speed | fast | ||||
L/D Ratio | 15 - 24:1 | ||||
Motor Oil Resistance | poor | ||||
Solvent Resistance | poor | ||||
UV-Ozone Stability | medium |