- 拉伸强度 [MPa]: 14.5
- 脆化温度 [℃]: -42.0
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.27 g/cc | 1.27 g/cc | ASTM D792 |
Mechanical Properties | Metric | English | Comments |
Hardness, Shore D | 45 | 45 | 10 Sec; ASTM D2240 |
Tensile Strength, Yield | 14.5 MPa | 2100 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
9.31 MPa @Strain 300 % | 1350 psi @Strain 300 % | Method A (Dumbbell & Section), 20 in/min; ASTM D412 | |
Elongation at Break | 550 % | 550 % | Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
Rebound | 36 % | 36 % | Bayshore; ASTM D2632 |
Tear Strength | 66.6 kN/m | 380 pli | Die C (graves), 20 in/min; ASTM D624 |
Thermal Properties | Metric | English | Comments |
Brittleness Temperature | -42.0 °C | -43.6 °F | ASTM D746 |
Flammability, UL94 | V-0 | V-0 | Natural, 0.062 in thick; UL 94 |
Oxygen Index | 27 % | 27 % | Limiting, 0.062 in bars; ASTM D2863 |