ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer

ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer 物性表: ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer物性表及特性介绍,ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer注塑参数详情,如需ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer下载, 可到相关下载区下载
  • 弯曲强度 [MPa]: 5.03
  • 脆化温度 [℃]: -35.0
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/cc23°C; ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8282Air at 257°F, 168 hr; ASTM D573
 8484.12 in; ASTM D2240
Tensile Strength at Break 7.4967 MPa1087.3 psi257°F, 70 hr in IRM 903 Oil; ASTM D471
 9.03 MPa1310 psiAcross Flow; ASTM D412
 10.387 MPa1506.5 psiAir at 257°F, 168 hr; ASTM D573
Tensile Strength, Ultimate 5.03 MPa730 psiAcross Flow; ASTM D412
Elongation at Break 227.7 %227.7 %257°F, 70 hr in IRM 903 Oil; ASTM D471
 244.2 %244.2 %Air at 257°F, 168 hr; ASTM D573
 330 %330 %Across Flow; ASTM D412
Tear Strength 34.0 kN/m194 pli73°C, Die C; ASTM D624
Compression Set 39 %39 %158°F, 22 hr; ASTM D395
 50 %50 %257°F, 70 hr; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -35.0 °C-31.0 °FASTM D746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 - 230 °C347 - 446 °F
Melt Temperature <= 102 °C<= 215 °F
 
Descriptive Properties
Change in Mass in IRM 903 Oil at 257°F for 70 hr0.48
ColorBlack
FormPellets

转载请注明: 转自中国塑胶原料之家 http://www.su-jiao.com/wuxingbiao/

本文链接: http://www.su-jiao.com/yuanliaoku/show-49429.html

免责声明: 本文 ExxonMobil Geolast® 701-87W183 Thermoplastic Elastomer 仅代表作者个人观点,中国塑胶原料之家无关。中国塑胶原料之家网所转载的内容,其版权均由原作者和资料提供方所拥有!如因作品版权问题需要处理,请与我们联络

塑胶原料之家,专业塑料网站、原料报价网站,免费发布塑胶供求信息。塑胶原料之家为您提供塑料供应、塑料求购、塑料行情、塑料展会、塑料原料资讯服务。

2008-2015 塑料|塑胶原料|物性表大全|UL黄卡|SGS报告查询|最新价格--塑胶原料之家

沪ICP备15027283号-4