颗粒样图:
物性表:
Physical Properties | Metric | English | Comments | ||
---|---|---|---|---|---|
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183/A | ||
Water Absorption | 0.90 % @Temperature 23.0 °C, Time 86400 sec |
0.90 % @Temperature 73.4 °F, Time 24.0 hour |
ISO 62 | ||
Linear Mold Shrinkage | 0.0071 cm/cm | 0.0071 in/in | Isotropy | ||
Linear Mold Shrinkage, Flow | 0.0060 cm/cm | 0.0060 in/in | |||
Linear Mold Shrinkage, Transverse | 0.0085 cm/cm | 0.0085 in/in | |||
Mechanical Properties | Metric | English | Comments | ||
Tensile Strength at Break | 150 MPa | 21800 psi | ISO 527 Type 1A | ||
Elongation at Break | 2.7 % | 2.7 % | ISO 527 Type 1A | ||
Tensile Modulus | 8.80 GPa | 1280 ksi | ISO 527 Type 1A | ||
Charpy Impact Unnotched | 5.50 J/cm² | 26.2 ft-lb/in² | ISO 179/1eU | ||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179/1eA | ||
Thermal Properties | Metric | English | Comments | ||
Melting Point | 263 °C | 505 °F | ISO 11357 | ||
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F | ISO 75/Af | ||
Processing Properties | Metric | English | Comments | ||
Feed Temperature | 270 - 275 °C | 518 - 527 °F | |||
Front Barrel Temperature | 285 - 290 °C | 545 - 554 °F | |||
Mold Temperature | 60.0 - 80.0 °C | 140 - 176 °F | |||
Drying Temperature | 80.0 °C | 176 °F | |||
Moisture Content | <= 0.20 % | <= 0.20 % | |||
De |
|||||
Compression Zone | 280-285°C |
应用:广泛用于制造机械、汽车、化学与电气装置的零件,如齿轮、滚子、滑轮、辊轴、泵体中叶轮、风扇叶片、高压密封围、阀座、垫片、衬套、各种把手、支撑架、电线包内层等。
上海松翰塑化科技有限公司,供应原料,品质真实,物实价廉。
PA6T,46,9T、PC、PC/ABS、PBT、ABS、PPA、PPS、POM、PMMA、TPE、PPO、LCP液晶聚合物。
欢迎各位客户前来咨询:
联系人: 夏先生
手 机:13501802636
QQ :205730283
邮 箱 :205730283@qq.com