机械性能(机械性能(Mechanical properties))值(Value)单位(Unit)测试标准(Test Standard)
ISO数据
拉伸模量(Tensile Modulus)3350MPaISO 527-1/-2
屈服应力(Yield stress)77MPaISO 527-1/-2
破坏时应变(Stress at break)62MPaISO 527-1/-2
破坏时应变(Strain at break)8%ISO 527-1/-2
简支梁缺口冲击强度(Charpy notched impact strength) (+23°C)2.7kJ/m²ISO 179/1eA
ASTM数据(ASTM Data)
悬臂梁式冲击切口 (1/8 in)0.032kJ/mASTM D 256
热性能(热性能(Thermal properties))值(Value)单位(Unit)测试标准(Test Standard)
ISO数据
熔化温度(熔化温度(Melting temperature)) (10°C/min)222°CISO 11357-1/-3
温度负荷变形(Temp. of deflection under load) (1.80 MPa)80°CISO 75-1/-2
温度负荷变形(Temp. of deflection under load) (0.45 MPa)190°CISO 75-1/-2
Vicat softening temperature A204°CISO 306
维卡软化温度(50℃/ h的50N)Vicat softening temperature200°CISO 306
COEFF线性热(Coeff. of linear therm. expansion) (parallel)80E-6/KISO 11359-1/-2
ASTM数据(ASTM Data)
UL 94 阻燃等级(Flame rating)V-0-UL 94
厚度测试(Thickness tested)0.97mm-
极限氧指数(Limiting 氧指数(Oxygen Index))29%ASTM D 2863
电气性能(Electrical properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据
体积电阻率(Volume resistivity)>1E13Ohm*mIEC 60093
电气强度(Electric strength)20kV/mmIEC 60243-1
相比漏电起痕指数(Comparative tracking index)600-IEC 60112
其他属性(Other properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据
吸水率(Water absorption)9%Sim. to ISO 62
密度(Density)1170kg/m³ISO 1183
CharacteristicsSpecial CharacteristicsFlame retardant, Heat stabilized or stable to heatFeaturesLow OdorRegional AvailabilityEuropeDisclaimerCopyright M-Base .

转载请注明: 转自中国塑胶原料之家 http://www.su-jiao.com/wuxingbiao/

本文链接: http://www.su-jiao.com/wuxingbiao/show-94569.html

免责声明: 本文 Taromid B 240 Y0|PA6|Taro Plast 仅代表作者个人观点,中国塑胶原料之家无关。中国塑胶原料之家网所转载的内容,其版权均由原作者和资料提供方所拥有!如因作品版权问题需要处理,请与我们联络

塑胶原料之家,专业塑料网站、原料报价网站,免费发布塑胶供求信息。塑胶原料之家为您提供塑料供应、塑料求购、塑料行情、塑料展会、塑料原料资讯服务。

2008-2015 塑料|塑胶原料|物性表大全|UL黄卡|SGS报告查询|最新价格--塑胶原料之家

沪ICP备15027283号-4