- 熔体流动速率 [g/10min]: 2.5
- 密度 [g/cm3]: 0.924
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.924 g/cc | 0.0334 lb/in³ | ASTM D1505 |
Vinyl Acetate Content | 2.5 % | 2.5 % | |
Thickness | 31.8 microns | 1.25 mil | |
Melt Flow | 2.5 g/10 min | 2.5 g/10 min | ASTM D1238 |
Antiblock Level | 1900 ppm | 1900 ppm | |
Slip Level | 1000 ppm | 1000 ppm | |
Mechanical Properties | Metric | English | Comments |
Film Elongation at Break, MD | 350 % | 350 % | ASTM D882 |
Film Elongation at Break, TD | 550 % | 550 % | ASTM D882 |
Elmendorf Tear Strength MD | 220 g | 220 g | ASTM D1922 |
Elmendorf Tear Strength TD | 250 g | 250 g | ASTM D1922 |
Dart Drop | 2.52 g/micron | 64.0 g/mil | F50; ASTM D1709 |
Film Tensile Strength at Break, MD | 22.8 MPa | 3300 psi | ASTM D882 |
Film Tensile Strength at Break, TD | 16.5 MPa | 2400 psi | ASTM D882 |
1% Secant Modulus, MD | 138 MPa | 20000 psi | ASTM E111 |
1% Secant Modulus, TD | 172 MPa | 25000 psi | ASTM E111 |
Thermal Properties | Metric | English | Comments |
Vicat Softening Point | 90.0 °C | 194 °F | ASTM D1525 |
Optical Properties | Metric | English | Comments |
Haze | 4.5 % | 4.5 % | ASTM D1003 |
Gloss | 73 % | 73 % | 45°; ASTM D2457 |
Processing Properties | Metric | English | Comments |
Melt Temperature | 191 °C | 375 °F | |
Die Opening | 0.0635 cm | 0.0250 in | |
Blow-up Ratio (BUR) | 2.0 | 2.0 |