- 熔体流动速率 [g/10min]: 3.2
Physical Properties | Metric | English | Comments | ||
---|---|---|---|---|---|
Melt Flow | 3.2 g/10 min @Load 2.16 kg, Temperature 230 °C | 3.2 g/10 min @Load 4.76 lb, Temperature 446 °F | ISO 1133 | ||
4.5 g/10 min @Load 5.00 kg, Temperature 190 °C | 4.5 g/10 min @Load 11.0 lb, Temperature 374 °F | ISO 1133 | |||
15 g/10 min @Load 5.00 kg, Temperature 230 °C | 15 g/10 min @Load 11.0 lb, Temperature 446 °F | ISO 1133 | |||
Mechanical Properties | Metric | English | Comments | ||
Film Elongation at Break, MD | 150 - 200 % | 150 - 200 % | ISO 527-3 | ||
Film Elongation at Break, TD | 50 - 90 % | 50 - 90 % | ISO 527-3 | ||
Tensile Modulus | 2.00 - 2.20 GPa | 290 - 319 ksi | MD; ISO 527-2 | ||
3.30 - 3.50 GPa | 479 - 508 ksi | TD; ISO 527-2 | |||
Film Tensile Strength at Break, MD | 130 - 160 MPa | 18900 - 23200 psi | ISO 527-3 | ||
Film Tensile Strength at Break, TD | 230 - 280 MPa | 33400 - 40600 psi | ISO 527-3 | ||
Thermal Properties | Metric | English | Comments | ||
Melting Point | 161 - 165 °C | 322 - 329 °F | DSC; ISO 3146 | ||
Optical Properties | Metric | English | Comments | ||
Haze | <= 1.0 % | <= 1.0 % | ASTM D1003 | ||
Gloss | >= 100 % | >= 100 % | 45°C of arc; ASTM D2457 | ||
Descriptive Properties | |||||
Isotactic Index (Heptane Insolubles, %) | 96 |