- 密度 [g/cm3]: 1.3
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.30 g/cc | 0.0470 lb/in³ | |
Mechanical Properties | Metric | English | Comments |
Elongation at Yield | 1.7 % | 1.7 % | |
Fracture Toughness | 1.62 MPa-m½ | 1.47 ksi-in½ | |
Thermal Properties | Metric | English | Comments |
Maximum Service Temperature, Air | 121 °C | 250 °F | |
Glass Transition Temp, Tg | 154 °C | 309 °F | Wet; RDS 7700 |
200 °C | 392 °F | Dry; RDS 7700 | |
Processing Properties | Metric | English | Comments |
Gel Time | 13.0 min @Temperature 177 °C | 13.0 min @Temperature 351 °F |