- 弯曲强度 [MPa]: 13.4
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 78 | 78 | Cured 10 min at 177°C and Post Cured 24 hr at 232°C |
Tensile Strength, Ultimate | 13.4 MPa | 1940 psi | Cured 10 min at 177°C and Post Cured 24 hr at 232°C |
Elongation at Break | 180 % | 180 % | Cured 10 min at 177°C and Post Cured 24 hr at 232°C |
50% Modulus | 0.00450 GPa | 0.653 ksi | Cured 10 min at 177°C and Post Cured 24 hr at 232°C |
100% Modulus | 0.00920 GPa | 1.33 ksi | Cured 10 min at 177°C and Post Cured 24 hr at 232°C |
Compression Set | 22 % @Temperature 200 °C | 22 % @Temperature 392 °F | Method B, O-rings, 70 hr |