- 拉伸强度 [MPa]: 24.14
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 66 | 66 | |
70 | 70 | heat aged 70 hours @ 100ºC | |
Tensile Strength, Yield | 24.14 MPa | 3501 psi | |
27.11 MPa | 3932 psi | heat aged 70 hours @ 100ºC | |
Elongation at Yield | 269.059 % | 269.059 % | heat aged 70 hours @ 100ºC |
289 % | 289 % | ||
100% Modulus | 0.00472 GPa | 0.684 ksi | |
200% Modulus | 0.0155 GPa | 2.25 ksi | |
Tear Strength | 51.0 kN/m | 291 pli | Die C |
Compression Set | 28.2 % @Temperature 100 °C, Time 79200 sec | 28.2 % @Temperature 212 °F, Time 22.0 hour | |
Processing Properties | Metric | English | Comments |
Cure Time | 7.00 min @Temperature 83.3 °C | 0.117 hour @Temperature 182 °F |