- 拉伸强度 [MPa]: 23.04
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Shore A | 80 | 80 | |
Tensile Strength, Yield | 23.04 MPa | 3341 psi | |
Elongation at Yield | 296 % | 296 % | |
100% Modulus | 0.00556 GPa | 0.807 ksi | |
200% Modulus | 0.01209 GPa | 1.754 ksi | |
Tear Strength | 35.4 kN/m | 202 pli | Die C |
Processing Properties | Metric | English | Comments |
Cure Time | 15.0 min @Temperature 160 °C | 0.250 hour @Temperature 320 °F |