Physical Properties | Metric | English | Comments | ||
---|---|---|---|---|---|
Viscosity | 10000 - 30000 cP @Temperature 40.0 °C | 10000 - 30000 cP @Temperature 104 °F | |||
Mechanical Properties | Metric | English | Comments | ||
Hardness, Shore A | 88 - 92 | 88 - 92 | |||
Tensile Strength at Break | 28.44 - 43.15 MPa | 4125 - 6258 psi | |||
Elongation at Break | 395 - 495 % | 395 - 495 % | |||
Tear Strength | 73.5 - 113 kN/m | 420 - 644 pli | |||
Processing Properties | Metric | English | Comments | ||
Processing Temperature | 100 °C | 212 °F | Working Temperature, Prepolymer | ||
Mold Temperature | 100 °C | 212 °F | |||
Pot Life | 11 min | 11 min | |||
Descriptive Properties | |||||
MOCA Temperature | 110°C | ||||
NCO Content | Max 4.4% | ||||
Min 4% | |||||
PHR of MOCA | 12.5% |