- 密度 [g/cm3]: 2.1
- 拉伸强度 [MPa]: 15.0
Physical Properties | Metric | English | Comments | ||
---|---|---|---|---|---|
Density | 2.10 g/cc | 0.0759 lb/in³ | ISO 1183-1 | ||
Mechanical Properties | Metric | English | Comments | ||
Hardness, Shore D | 67 | 67 | DIN 53505 | ||
Tensile Strength, Yield | 15.0 MPa | 2180 psi | ISO 527-1/-2 | ||
Elongation at Break | 180 % | 180 % | ISO 527-1/-2 | ||
Modulus of Elasticity | 1.27 GPa | 184 ksi | |||
Compressive Yield Strength | 10.0 MPa @Strain 1.00 % | 1450 psi @Strain 1.00 % | dry; ISO 604 | ||
Charpy Impact, Notched | 0.800 J/cm² | 3.81 ft-lb/in² | ISO 179-1/1eA | ||
Coefficient of Friction, Dynamic | 0.12 | 0.12 | |||
Sand Slurry | 1.0 | 1.0 | µm/km | ||
Electrical Properties | Metric | English | Comments | ||
Electrical Resistivity | 1000 - 1.00e+6 ohm-cm | 1000 - 1.00e+6 ohm-cm | IEC 60093 | ||
Surface Resistance | 1000 - 1.00e+6 ohm | 1000 - 1.00e+6 ohm | IEC 60093 | ||
Thermal Properties | Metric | English | Comments | ||
CTE, linear | 95.0 µm/m-°C @Temperature 23.0 - 100 °C | 52.8 µin/in-°F @Temperature 73.4 - 212 °F | |||
Melting Point | 330 °C | 626 °F | ISO 11357-1 | ||
Maximum Service Temperature, Air | 260 °C @Time 7.20e+7 sec | 500 °F @Time 20000 hour | |||
300 °C @Time <=86400 sec | 572 °F @Time <=24.0 hour | ||||
Minimum Service Temperature, Air | -200 °C | -328 °F | |||
Glass Transition Temp, Tg | 127 °C | 261 °F | ISO 11357-1 | ||
Flammability, UL94 | V-0 | V-0 | |||
Compliance Properties | Metric | English | Comments | ||
FDA | No | No | |||
Descriptive Properties | |||||
Color | Black |