Physical Properties | Metric | English | Comments | ||
---|---|---|---|---|---|
Specific Gravity | 1.14 g/cc | 1.14 g/cc | ASTM D792 | ||
Mechanical Properties | Metric | English | Comments | ||
Hardness, Shore A | 58 | 58 | 10 sec; ASTM D2240 | ||
Tensile Strength at Break | 11.0 MPa | 1600 psi | ASTM D412 | ||
Elongation at Break | 680 % | 680 % | ASTM D412 | ||
Tear Strength | 40.3 kN/m | 230 pli | ASTM D412 | ||
Taber Abrasion, mg/1000 Cycles | 60 | 60 | ASTM D1044 | ||
Compression Set | 18 % @Temperature 22.8 °C, Time 79200 sec | 18 % @Temperature 73.0 °F, Time 22.0 hour | |||
84 % @Temperature 120 °C, Time 79200 sec | 84 % @Temperature 248 °F, Time 22.0 hour | ||||
Tensile Set | 10 % | 10 % | 1; ASTM D412 | ||
34 % | 34 % | 3; ASTM D412 | |||
60 % | 60 % | At Break; ASTM D412 | |||
60 % | 60 % | ASTM D412 | |||
Processing Properties | Metric | English | Comments | ||
Rear Barrel Temperature | 180 °C | 356 °F | |||
Middle Barrel Temperature | 190 °C | 374 °F | |||
Front Barrel Temperature | 200 °C | 392 °F | |||
Nozzle Temperature | 205 °C | 401 °F | |||
Mold Temperature | 10.0 - 30.0 °C | 50.0 - 86.0 °F | |||
Drying Temperature | 80.0 °C | 176 °F | |||
Dry Time | 2 - 4 hour | 2 - 4 hour | |||
Descriptive Properties | |||||
Injection Rate | Fast |