流变性能(Rheological properties)dry / cond单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
熔体体积流动速率(Melt volume-flow rate) (MVR)20 / *cm³/10minISO 1133
温度(Temperature)275 / *°CISO 1133
负载(Load)5 / *kgISO 1133
成型收缩(Molding shrinkage) (parallel)0.4 / *%ISO 294-4, 2577
成型收缩(Molding shrinkage) (normal)1.0 / *%ISO 294-4, 2577
机械性能(机械性能(Mechanical properties))dry / cond单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
拉伸模量(Tensile Modulus)11500 / 8500MPaISO 527-1/-2
破坏时应变(Stress at break)210 / 150MPaISO 527-1/-2
破坏时应变(Strain at break)3 / 5%ISO 527-1/-2
Tensile creep modulus (1h)* / 7450MPaISO 899-1
Tensile creep modulus (1000h)* / 6600MPaISO 899-1
简支梁冲击强度(Charpy impact strength) (+23°C)95 / 105kJ/m²ISO 179/1eU
简支梁冲击强度(Charpy impact strength) (-30°C)75 / -kJ/m²ISO 179/1eU
简支梁缺口冲击强度(Charpy notched impact strength) (+23°C)14 / 22kJ/m²ISO 179/1eA
简支梁缺口冲击强度(Charpy notched impact strength) (-30°C)12 / -kJ/m²ISO 179/1eA
热性能(热性能(Thermal properties))dry / cond单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
熔化温度(熔化温度(Melting temperature)) (10°C/min)260 / *°CISO 11357-1/-3
温度负荷变形(Temp. of deflection under load) (1.80 MPa)250 / *°CISO 75-1/-2
温度负荷变形(Temp. of deflection under load) (0.45 MPa)250 / *°CISO 75-1/-2
维卡软化温度(50℃/ h的50N)Vicat softening temperature250 / *°CISO 306
COEFF线性热(Coeff. of linear therm. expansion) (parallel)17.5 / *E-6/KISO 11359-1/-2
COEFF线性热(Coeff. of linear therm. expansion) (normal)65 / *E-6/KISO 11359-1/-2
燃烧性(球压痕硬度(Burning behav)). at 1.5 mm nom. thickn.HB / *classIEC 60695-11-10
厚度测试(Thickness tested)1.5 / *mmIEC 60695-11-10
UL 识别(recognition)UL / *--
燃烧性(球压痕硬度(Burning behav)). at thickness hHB / *classIEC 60695-11-10
厚度测试(Thickness tested)0.7 / *mmIEC 60695-11-10
UL 识别(recognition)UL / *--
Oxygen index24 / *%ISO 4589-1/-2
电气性能(Electrical properties)dry / cond单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
相对介电常数(Relative permittivity) (1MHz)3.5 / 5.7-IEC 60250
耗散因数(耗散因数(Dissipation factor)) (100Hz)200 / 3000E-4IEC 60250
耗散因数(耗散因数(Dissipation factor)) (1MHz)200 / 3000E-4IEC 60250
体积电阻率(Volume resistivity)1E13 / 1E10Ohm*mIEC 60093
表面电阻率(Surface resistivity)* / 1E10OhmIEC 60093
电气强度(Electric strength)40 / 34kV/mmIEC 60243-1
相比漏电起痕指数(Comparative tracking index)- / 450-IEC 60112
其他属性(Other properties)dry / cond单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
吸水率(Water absorption)5 / *%Sim. to ISO 62
吸湿性(Humidity absorption)1.6 / *%Sim. to ISO 62
密度(Density)1410 / -kg/m³ISO 1183
材料特殊性能(Material specific properties)dry / cond单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
粘数(Viscosity number)145 / *cm³/gISO 307, 1157, 1628
流变计算属性(Rheological calculation properties)值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
喷射温度(Ejection temperature)195°C-
Test specimen production值(Value)单位(Unit)测试标准(Test Standard)
ISO数据(ISO数据(CAMPUS/ISO) Data)
Injection Molding, melt temperature290°CISO 294
Injection Molding, mold temperature80°CISO 10724
Injection Molding, injection velocity200mm/sISO 294
Diagrams allowed water content: .15 % ISO 1817 Liquid F) (23°C)
ISO 1817 Liquid F) (>90°C)
Salt solutions
4 Brake fluid (130°C)
.

转载请注明: 转自中国塑胶原料之家 http://www.su-jiao.com/wuxingbiao/

本文链接: http://www.su-jiao.com/wuxingbiao/show-82644.html

免责声明: 本文 Ultramid® A3WG7|PA66-GF35|BASF 仅代表作者个人观点,中国塑胶原料之家无关。中国塑胶原料之家网所转载的内容,其版权均由原作者和资料提供方所拥有!如因作品版权问题需要处理,请与我们联络

塑胶原料之家,专业塑料网站、原料报价网站,免费发布塑胶供求信息。塑胶原料之家为您提供塑料供应、塑料求购、塑料行情、塑料展会、塑料原料资讯服务。

2008-2015 塑料|塑胶原料|物性表大全|UL黄卡|SGS报告查询|最新价格--塑胶原料之家

沪ICP备15027283号-4