- 密度 [g/cm3]: 1.15
- 透光率 [%]: 92.0
Physical Properties | Metric | English | Comments | ||
---|---|---|---|---|---|
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 | ||
Mechanical Properties | Metric | English | Comments | ||
Film Tensile Strength at Yield, MD | 50.0 MPa | 7250 psi | no direction given; ISO 527 | ||
Film Elongation at Break, MD | 30 % | 30 % | no direction given; ISO 527 | ||
Film Elongation at Yield, MD | 4.5 % | 4.5 % | no direction given; ISO 527 | ||
Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 | ||
Electrical Properties | Metric | English | Comments | ||
Volume Resistivity | >= 1.00e+13 ohm-cm | >= 1.00e+13 ohm-cm | No thickness given; IEC 250 | ||
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 250 | ||
Dissipation Factor | 0.030 @Frequency 1e+6 Hz | 0.030 @Frequency 1e+6 Hz | IEC 250 | ||
0.040 @Frequency 100 Hz | 0.040 @Frequency 100 Hz | IEC 250 | |||
Thermal Properties | Metric | English | Comments | ||
CTE, linear | 110 µm/m-°C @Temperature 0.000 - 50.0 °C | 61.1 µin/in-°F @Temperature 32.0 - 122 °F | DIN 53752A | ||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |||
Vicat Softening Point | 98.0 °C | 208 °F | ISO 306, Method B 50 | ||
Optical Properties | Metric | English | Comments | ||
Refractive Index | 1.49 | 1.49 | ISO 489 | ||
Haze | <= 1.5 % | <= 1.5 % | ASTM D1003 | ||
Yellow Index | <= 1.0 % | <= 1.0 % | ASTM D1925 | ||
Transmission, Visible | 92 % | 92 % | DIN 5036 | ||
Descriptive Properties | |||||
Pencil Hardness | 1H-2H | ASTM D3363 |