Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2000 cP @Temperature 25.0 °C | 2000 cP @Temperature 77.0 °F | |
Mechanical Properties | Metric | English | Comments |
Hardness, Shore D | 85 | 85 | |
Electrical Properties | Metric | English | Comments |
Volume Resistivity | <= 4.00e+14 ohm-cm | <= 4.00e+14 ohm-cm | |
Dielectric Constant | 4.1 @Frequency 1000 Hz | 4.1 @Frequency 1000 Hz | |
Dielectric Strength | 15.0 kV/mm | 380 kV/in | |
Dissipation Factor | 0.0080 @Frequency 1000 Hz | 0.0080 @Frequency 1000 Hz | |
Thermal Properties | Metric | English | Comments |
Maximum Service Temperature, Air | 155 °C | 311 °F | |
Processing Properties | Metric | English | Comments |
Cure Time | >= 180 min | >= 3.00 hour | Value for cure at 130°C |
Pot Life | 60 min | 60 min | Value for 100 grams at 40°C |
480 min | 480 min | Value for 100 grams at 25°C |