Physical Properties | Metric | English | Comments | ||
---|---|---|---|---|---|
Specific Gravity | 1.65 - 2.15 g/cc | 1.65 - 2.15 g/cc | ASTM D792 | ||
Mechanical Properties | Metric | English | Comments | ||
Hardness, Shore A | 58 - 72 | 58 - 72 | ASTM D2240 | ||
Tensile Strength at Break | >= 1.38 MPa | >= 200 psi | ASTM D412 | ||
Elongation at Break | 100 - 300 % | 100 - 300 % | ASTM D412 | ||
Tear Strength | 5.250 kN/m | 29.96 pli | ASTM D624 | ||
Compression Set | >= 30 % @Temperature 100 °C, Time 252000 sec | >= 30 % @Temperature 212 °F, Time 70.0 hour | ASTM D395 Method B | ||
Electrical Properties | Metric | English | Comments | ||
Volume Resistivity | 0.010 ohm-cm | 0.010 ohm-cm | as supplied without pressure sensitive adhesive; MIL-DTL-83528 | ||
0.010 ohm-cm | 0.010 ohm-cm | Post Tensile Set; MIL-DLT-83528 Para.4.6.9 | |||
Shielding Effectiveness | >= 100 dB | >= 100 dB | 100 MHz (E Field); MIL-G-83528 | ||
>= 50 dB @Frequency 200000 Hz | >= 50 dB @Frequency 200000 Hz | H Field; MIL-DTL-83528 Para.4.6.12 | |||
>= 75 dB @Frequency 4.00e+10 Hz | >= 75 dB @Frequency 4.00e+10 Hz | Plane Wave; MIL-DTL-83528 Para.4.6.12 | |||
>= 80 dB @Frequency 1.00e+10 Hz | >= 80 dB @Frequency 1.00e+10 Hz | Plane Wave; MIL-DTL-83528 Para.4.6.12 | |||
>= 90 dB @Frequency 2.00e+9 Hz | >= 90 dB @Frequency 2.00e+9 Hz | Plane Wave; MIL-DTL-83528 Para.4.6.12 | |||
>= 100 dB @Frequency 1.00e+8 Hz | >= 100 dB @Frequency 1.00e+8 Hz | E Field; MIL-DTL-83528 Para.4.6.12 | |||
>= 100 dB @Frequency 5.00e+8 Hz | >= 100 dB @Frequency 5.00e+8 Hz | E Field; MIL-DTL-83528 Para.4.6.12 | |||
Thermal Properties | Metric | English | Comments | ||
Thermal Conductivity | 1.20 W/m-K @Pressure 2.07 MPa | 8.33 BTU-in/hr-ft²-°F @Pressure 300 psi | ASTM D5470 | ||
Maximum Service Temperature, Air | 160 °C | 320 °F | |||
Minimum Service Temperature, Air | -55.0 °C | -67.0 °F | Flex TR10; ASTM D1329 | ||
Descriptive Properties | |||||
Binder | Silicone | ||||
Filler | Ag/Glass | ||||
Heat Aging ohm-cm max | 0.01 | ||||
Type | M | MIL-DTL-83528 |