- 熔体流动速率 [g/10min]: 0.5
- 密度 [g/cm3]: 0.926
Physical Properties | Metric | English | Comments | ||
---|---|---|---|---|---|
Density | 0.926 g/cc | 0.0335 lb/in³ | ASTM D1505 | ||
Vinyl Acetate Content | 6.6 % | 6.6 % | |||
Thickness | 50.8 microns | 2.00 mil | 2:1 BUR; 25 mil die gap | ||
Melt Flow | 0.50 g/10 min | 0.50 g/10 min | ASTM D1238 | ||
Mechanical Properties | Metric | English | Comments | ||
Film Elongation at Break, MD | 500 % | 500 % | ASTM D882 | ||
Film Elongation at Break, TD | 600 % | 600 % | ASTM D882 | ||
Elmendorf Tear Strength MD | 140 g | 140 g | ASTM D1922 | ||
Elmendorf Tear Strength TD | 260 g | 260 g | ASTM D1922 | ||
Dart drop Test | 310 g | 0.684 lb | F50; ASTM D1709 | ||
Film Tensile Strength at Break, MD | 26.2 MPa | 3800 psi | ASTM D882 | ||
Film Tensile Strength at Break, TD | 24.8 MPa | 3600 psi | ASTM D882 | ||
1% Secant Modulus, MD | 117 MPa | 17000 psi | ASTM D882 | ||
1% Secant Modulus, TD | 145 MPa | 21000 psi | ASTM D882 | ||
Thermal Properties | Metric | English | Comments | ||
Vicat Softening Point | 87.0 °C | 189 °F | ASTM D1525 | ||
Processing Properties | Metric | English | Comments | ||
Melt Temperature | 221 °C | 430 °F | |||
Descriptive Properties | |||||
Antiblock | High | ||||
Slip | High |