- 熔体流动速率 [g/10min]: 3.0
- 密度 [g/cm3]: 1.36
- 弯曲模量 [MPa]: 4.75
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.36 g/cc | 0.0491 lb/in³ | STN EN ISO 1183-1 |
Filler Content | 15 % | 15 % | Glass Beads |
15 % | 15 % | Glass Fibers | |
Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | STN EN ISO 294-4 |
Linear Mold Shrinkage, Transverse | 0.0060 cm/cm | 0.0060 in/in | STN EN ISO 294-4 |
Melt Flow | 3.0 g/10 min @Load 0.325 kg, Temperature 275 °C | 3.0 g/10 min @Load 0.716 lb, Temperature 527 °F | STN EN ISO 1133 |
Mechanical Properties | Metric | English | Comments |
Tensile Strength at Break | 115 MPa | 16700 psi | STN EN ISO 527-2 |
Elongation at Break | 3.5 % | 3.5 % | STN EN ISO 527-2 |
Tensile Modulus | 5.80 GPa | 841 ksi | STN EN ISO 527-2 |
Flexural Strength | 165 MPa | 23900 psi | STN EN ISO 178 |
Flexural Modulus | 4.75 GPa | 689 ksi | STN EN ISO 178 |
Charpy Impact Unnotched | 4.00 J/cm² @Temperature -20.0 °C | 19.0 ft-lb/in² @Temperature -4.00 °F | STN EN ISO 179 |
4.50 J/cm² @Temperature 23.0 °C | 21.4 ft-lb/in² @Temperature 73.4 °F | STN EN ISO 179 | |
Charpy Impact, Notched | 0.300 J/cm² @Temperature -20.0 °C | 1.43 ft-lb/in² @Temperature -4.00 °F | STN EN ISO 179 |
0.550 J/cm² @Temperature 23.0 °C | 2.62 ft-lb/in² @Temperature 73.4 °F | STN EN ISO 179 | |
Thermal Properties | Metric | English | Comments |
Melting Point | 262 °C | 504 °F | STN EN 11357-1 |
Deflection Temperature at 1.8 MPa (264 psi) | 245 °C | 473 °F | STN EN ISO 75-2 (A) |
Vicat Softening Point | 240 °C | 464 °F | STN EN ISO 306 |
Flammability, UL94 | HB | HB | |
Glow Wire Test | 650 °C @Thickness 3.00 mm | 1200 °F @Thickness 0.118 in | STN EN 60695-2-12 |
Processing Properties | Metric | English | Comments |
Melt Temperature | 250 - 270 °C | 482 - 518 °F | |
Mold Temperature | 70.0 - 90.0 °C | 158 - 194 °F | |
Drying Temperature | 80.0 °C @Time 14400 sec | 176 °F @Time 4.00 hour | |
Moisture Content | 0.10 % | 0.10 % | STN EN ISO 3344 |
Injection Pressure | 70.0 - 120 MPa | 10200 - 17400 psi |