  • 吸水率 [%]: 0.8
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D1505
Water Absorption 0.80 %0.80 %Extractable Content
 1.6 %1.6 %in 24 hours
Moisture Absorption at Equilibrium 2.7 %2.7 %at 50% RH
Water Absorption at Saturation 9.5 %9.5 %
Oxygen Transmission Rate 40.3 cc/m²/day2.60 cc/100 in²/day
Nitrogen Transmission 14.0 cc-mm/m²-24hr-atm35.6 cc-mil/100 in²-24hr-atmcc/m²/day, No thickness given
Carbon Dioxide Transmission 72.8 cc-mm/m²-24hr-atm185 cc-mil/100 in²-24hr-atmcc/m²/day, No thickness given
Viscosity Measurement 205205FAV; ASTM D789
Maximum Moisture Content 0.0800.080
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FASTM D3418
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 230 - 260 °C446 - 500 °FCast Film
 246 - 254 °C475 - 489 °FTubular (Blown) Film
Adapter Temperature 260 °C500 °FTubular (Blown) Film
 260 - 266 °C500 - 511 °FCast Film
Die Temperature 254 °C490 °FTubular (Blown) Film
 260 °C500 °FCast Film
Melt Temperature 254 - 260 °C489 - 500 °FTubular (Blown) Film
 260 - 270 °C500 - 518 °FCast Film
Moisture Content 0.070 %0.070 %

转载请注明: 转自中国塑胶原料之家 http://www.su-jiao.com/wuxingbiao/

本文链接: http://www.su-jiao.com/yuanliaoku/show-45883.html

免责声明: 本文 Honeywell Aegis™ H205QP Nylon 6 Extrusion Grade Homopolymer Film 仅代表作者个人观点,中国塑胶原料之家无关。中国塑胶原料之家网所转载的内容,其版权均由原作者和资料提供方所拥有!如因作品版权问题需要处理,请与我们联络

塑胶原料之家,专业塑料网站、原料报价网站,免费发布塑胶供求信息。塑胶原料之家为您提供塑料供应、塑料求购、塑料行情、塑料展会、塑料原料资讯服务。

2008-2015 塑料|塑胶原料|物性表大全|UL黄卡|SGS报告查询|最新价格--塑胶原料之家

沪ICP备15027283号-4