- 拉伸强度 [MPa]: 6.14
- 脆化温度 [℃]: -54.0
Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.26 g/cc | 1.26 g/cc | ASTM D792 |
Mechanical Properties | Metric | English | Comments |
Hardness, Shore A | 65 | 65 | Instant; ASTM D2240 |
Tensile Strength, Yield | 6.14 MPa | 890 psi | Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412 |
3.45 MPa @Strain 300 % | 500 psi @Strain 300 % | Method A (Dumbbell & Section), 20 in/min; ASTM D412 | |
Elongation at Break | 600 % | 600 % | Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
Rebound | 41 % | 41 % | Bayshore; ASTM D2632 |
Tear Strength | 29.8 kN/m | 170 pli | Die C (graves), 20 in/min; ASTM D624 |
Compression Set | 19 % | 19 % | Method B, 73°F(23°C), 22 hrs; ASTM D395 |
Thermal Properties | Metric | English | Comments |
Brittleness Temperature | -54.0 °C | -65.2 °F | ASTM D746 |
Flammability, UL94 | V-0 | V-0 | Natural, 0.062 in thick; UL 94 |
Oxygen Index | 27 % | 27 % | Limiting, 0.062 in bars; ASTM D2863 |