- 拉伸强度 [MPa]: 2.8
Physical Properties | Metric | English | Comments | ||
---|---|---|---|---|---|
Specific Gravity | 1.12 g/cc | 1.12 g/cc | Base | ||
Viscosity | 20000 cP | 20000 cP | catalyzed with Stretch Effect B | ||
25000 cP | 25000 cP | Base | |||
Mechanical Properties | Metric | English | Comments | ||
Hardness, Shore A | 22 | 22 | cured | ||
Tensile Strength, Yield | >= 2.80 MPa | >= 406 psi | cured | ||
Elongation at Break | >= 1200 % | >= 1200 % | cured | ||
Tear Strength | >= 17.5 kN/m | >= 100 pli | cured | ||
Thermal Properties | Metric | English | Comments | ||
Maximum Service Temperature, Air | 204 °C | 399 °F | |||
Minimum Service Temperature, Air | -60.0 °C | -76.0 °F | |||
Processing Properties | Metric | English | Comments | ||
Dry Time | 8 - 12 hour | 8 - 12 hour | Demold time, catalyzed with Stretch Effect B | ||
Pot Life | >= 90 min | >= 90 min | catalyzed with Stretch Effect B | ||
Descriptive Properties | |||||
Color | Translucent | catalyzed with Stretch Effect B | |||
Translucent | Base | ||||
Linear Shrinkage, inches, max | 0.1 |
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.