Parker Chomerics CHO-SEAL 1215 Conductive Elastomer

Parker Chomerics CHO-SEAL 1215 Conductive Elastomer 物性表: Parker Chomerics CHO-SEAL 1215 Conductive Elastomer物性表及特性介绍,Parker Chomerics CHO-SEAL 1215 Conductive Elastomer注塑参数详情,如需Parker Chomerics CHO-SEAL 1215 Conductive Elastomer下载, 可到相关下载区下载
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.05 - 3.95 g/cc3.05 - 3.95 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 58 - 7258 - 72
Tensile Strength at Break >= 1.38 MPa>= 200 psiASTM D412
Elongation at Break 100 - 300 %100 - 300 %ASTM D412
Tear Strength 4.38 - 7.01 kN/m25.0 - 40.0 pliASTM D624
Compression Set <= 32 %
@Temperature 100 °C,
Time 252000 sec
<= 32 %
@Temperature 212 °F,
Time 70.0 hour
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0040 ohm-cm0.0040 ohm-cmas supplied without pressure sensitive adhesive; MIL-DLT-83528
 0.0080 ohm-cm0.0080 ohm-cmPost Tensile Set; MIL-DLT-83528
Shielding Effectiveness  >= 70 dB
@Frequency 200000 Hz
>= 70 dB
@Frequency 200000 Hz
H Field; MIL-DLT-83528 Para.4.6.12
 >= 90 dB
@Frequency 4.00e+10 Hz
>= 90 dB
@Frequency 4.00e+10 Hz
Plane Wave; MIL-DLT-83528 Para.4.6.12
 >= 120 dB
@Frequency 1.00e+8 Hz
>= 120 dB
@Frequency 1.00e+8 Hz
E Field; MIL-DLT-83528 Para.4.6.12
 >= 120 dB
@Frequency 5.00e+8 Hz
>= 120 dB
@Frequency 5.00e+8 Hz
E Field; MIL-DLT-83528 Para.4.6.12
 >= 120 dB
@Frequency 2.00e+9 Hz
>= 120 dB
@Frequency 2.00e+9 Hz
Plane Wave; MIL-DLT-83528 Para.4.6.12
 >= 120 dB
@Frequency 1.00e+10 Hz
>= 120 dB
@Frequency 1.00e+10 Hz
Plane Wave; MIL-DLT-83528 Para.4.6.12
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 2.10 W/m-K
@Pressure 2.07 MPa
14.6 BTU-in/hr-ft²-°F
@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -65.0 °C-85.0 °FTR10; ASTM D1329
 
Descriptive Properties
BinderSilicone
EMP Survivability>0.9 kA / inMIL-DTL-83528 Para.4.6.16
FillerAg/Cu
Heat Aging <0.01ohm-cmMIL-DTL-83528 Para.4.6.15
TypeAMIL-DTL-83528
Vibration Resistance, After <0.004 ohm-cmMIL-DTL-83528 Para.4.6.13
Vibration Resistance, During <0.006 ohm-cmMIL-DTL-83528 Para.4.6.13

转载请注明: 转自中国塑胶原料之家 http://www.su-jiao.com/wuxingbiao/

本文链接: http://www.su-jiao.com/yuanliaoku/show-35822.html

免责声明: 本文 Parker Chomerics CHO-SEAL 1215 Conductive Elastomer 仅代表作者个人观点,中国塑胶原料之家无关。中国塑胶原料之家网所转载的内容,其版权均由原作者和资料提供方所拥有!如因作品版权问题需要处理,请与我们联络

塑胶原料之家,专业塑料网站、原料报价网站,免费发布塑胶供求信息。塑胶原料之家为您提供塑料供应、塑料求购、塑料行情、塑料展会、塑料原料资讯服务。

2008-2015 塑料|塑胶原料|物性表大全|UL黄卡|SGS报告查询|最新价格--塑胶原料之家

沪ICP备15027283号-4