- 熔体流动速率 [g/10min]: 2.0
- 密度 [g/cm3]: 0.925
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.925 g/cc | 0.0334 lb/in³ | ASTM D792 |
Thickness | 50.8 microns | 2.00 mil | |
Melt Flow | 2.0 g/10 min | 2.0 g/10 min | ASTM D1238 |
Mechanical Properties | Metric | English | Comments |
Film Tensile Strength at Yield, MD | 10.96 MPa | 1589 psi | ASTM D882 |
Film Tensile Strength at Yield, TD | 10.44 MPa | 1514 psi | ASTM D882 |
Film Elongation at Break, MD | 669 % | 669 % | ASTM D882 |
Film Elongation at Break, TD | 787 % | 787 % | ASTM D882 |
Impact | 271 | 271 | [ft-lbf/in3]; Puncture Resistance; Dow Method |
1575 | 1575 | [ft-lbf/in3]; Toughness MD; ASTM D882 | |
1670 | 1670 | [ft-lbf/in3]; Toughness TD; ASTM D882 | |
Elmendorf Tear Strength MD | 650 g | 650 g | ASTM D1922 |
Elmendorf Tear Strength TD | 957 g | 957 g | ASTM D1922 |
Elmendorf Tear Strength, MD | 12.8 g/micron | 325 g/mil | ASTM D1922 |
Elmendorf Tear Strength, TD | 18.84 g/micron | 478.5 g/mil | ASTM D1922 |
Dart drop Test | 182 g | 0.401 lb | Method A; ASTM D1709 |
Film Tensile Strength at Break, MD | 48.72 MPa | 7066 psi | ASTM D882 |
Film Tensile Strength at Break, TD | 40.40 MPa | 5859 psi | ASTM D882 |
Thermal Properties | Metric | English | Comments |
Melting Point | 124 °C | 255 °F | Dow Method (DSC) |
Vicat Softening Point | 108 °C | 226 °F | ASTM D1525 |
Optical Properties | Metric | English | Comments |
Haze | 3.7 % | 3.7 % | ASTM D1003 |
Gloss | 90.5 % | 90.5 % | 45°; ASTM D2457 |